Prototype to measure bracket debonding force in vivo

Jéssika Lagni TONUS, Fernanda Borguetti MANFROI, Gilberto Antonio BORGES, Eduardo Correa GRIGOLO, Sérgio HELEGDA, Ana Maria SPOHR

Introduction: Material biodegradation that occurs in the mouth may interfere in the bonding strength between the bracket and the enamel, causing lower bond strength values in vivo, in comparison with in vitro studies. Objective: To develop a prototype to measure bracket debonding force in vivo and to evaluate, in vitro, the bond strength obtained with the prototype. Methods: A original plier (3M Unitek) was modified by adding one strain gauge directly connected to its claw. An electronic circuit performed the reading of the strain gauge, and the software installed in a computer recorded the values of the bracket debonding force, in kgf. Orthodontic brackets were bonded to the facial surface of 30 bovine incisors with adhesive materials. In Group 1 (n = 15), debonding was carried out with the prototype, while tensile bond strength testing was performed in Group 2 (n = 15). A universal testing machine was used for the second group. The adhesive remnant index (ARI) was recorded. Results: According to Student’s t test (α = 0.05), Group 1 (2.96 MPa) and Group 2 (3.08 MPa) were not significantly different. ARI score of 3 was predominant in the two groups. Conclusion: The prototype proved to be reliable for obtaining in vivo bond strength values for orthodontic brackets.

Keywords: Brackets. Bond strength. Enamel.

How to cite: Tonus JL, Manfroi FB, Borges GA, Grigolo EC, Helegda S, Spohr AM. Prototype to measure bracket debonding force in vivo. Dental Press J Orthod. 2017 Jan-Feb;22(1):82-8. DOI: http://dx.doi.org/10.1590/2177-6709.22.1.082-088.oar

Friday, April 19, 2024 01:13